聚丙烯酸接枝碱木质素/酚醛开孔吸水材料的工艺研究

杨伟, 李追, 毕严文, 路进程, 龚承承, 曹伟华, 方桂珍, 马艳丽   

  1. 东北林业大学 材料科学与工程学院, 黑龙江 哈尔滨 150040
  • 收稿日期:2014-06-30 修回日期:2015-02-14 出版日期:2015-05-30 发布日期:2015-08-04
  • 通讯作者: 马艳丽,女,讲师,博士,研究领域:木材化学、生物质复合材料;E-mail:myl219@126.com。 E-mail:myl219@126.com
  • 作者简介:杨伟(1992—),男,云南绥江人,本科生,主要从事生物质复合功能材料的研究
  • 基金资助:
    黑龙江省自然科学基金青年基金 (QC2014C011);中央高校基本科研业务费专项资金资助(DL13CB09);大学生科研训练项目(KY2013003)

Preparation Technology of Polyacrylic Acid Grafted Alkali Lignin/ Phenolic Open-cell Absorbent Material

YANG Wei, LI Zhui, BI Yan-wen, LU Jin-cheng, GONG Cheng-cheng, CAO Wei-hua, FANG Gui-zhen, MA Yan-li   

  1. College of Material Science and Engineering, Northeast Forestry University, Harbin 150040, China
  • Received:2014-06-30 Revised:2015-02-14 Online:2015-05-30 Published:2015-08-04

摘要: 利用聚丙烯酸接枝碱木质素(PAA-g-AL)和酚醛树脂(PF)制备聚丙烯酸接枝碱木质素/酚醛开孔吸水材料(PAA-g-AL/PF),并对PAA-g-AL、发泡剂、表面活性剂、增韧剂加入量和发泡温度的影响进行了研究。采用SEM、FT-IR、DSC和TGA分别对PAA-g-AL/PF的微观形貌、官能团和热性能进行表征。结果表明,50 g PF加入7%聚丙烯酸接枝碱木质素、16%发泡剂、8%表面活性剂、7%增韧剂和4.8 g 10%盐酸在发泡温度为62 ℃的条件下2 h发泡成型制得的PAA-g-AL/PF开孔吸水材料,吸水率达33.08 g/g、表观密度为5.1 g/dm3,PAA-g-AL与PF网络之间存在显著的分子间氢键作用,136 ℃以下热稳定性良好且材料为均匀开孔结构,吸水后形状保持不变。

关键词: 聚丙烯酸接枝碱木质素, 酚醛树脂, 开孔, 吸水材料

Abstract: Polyacrylic acid grafted alkali lignin/phenolic foam materials (PAA-g-AL/PF) was prepared by using polyacrylic acid grafted alkali lignin and phenolic resin.The influences of preparation conditions such as the additions of foaming agent, surfactant, toughening agent, the foaming temperature on their properties were studied.The morphology, functional groups, and thermal properties of PAA-g-AL/PF were investigated by SEM, FT-IR, DSC, and TGA.It was found that the optimum conditions to prepare PAA-g-AL/PF open-cell absorbent material were 50 g PF with the additions of PAA-g-AL 7%, foaming agent 16%, surfactant 8%, toughening agent 7%, 4.8g 10% hydrochloric acid solution, and the foaming temperature 62 ℃.Under these conditions, the water absorption of PAA-g-AL/PF was 33.08 g/g, the apparent density was 5.1 g/dm3, and it was thermally stable under 136 ℃.The obtained PAA-g-AL/PF was a uniform open-cell material and keeping its shape after absorbing water.

Key words: polyacrylic acid grafted alkali lignin, phenolic resin, open-cell, absorbent materials